A182 F60

Spread the love

Identification Symbol: A182 F60

UNS Designation: S32205

Type: Ferritic – Austenitic Stainless Steel

Heat Treatment: Solution Treat and Quench

 

Chemical Requirements  Composition, max, %

Elements A182 F60
Carbon 0.030
Manganese 1.50
Phosphorus 0.030
Sulfur 0.020
Silicon 1.00
Nickel 4.5-6.5
Chromium 22.0-23.0
Molybdenum 3.0-3.5
Nitrogen 0.14-0.20

 

Tensile and Hardness Requirements

Grade Symbol F60
Tensile Strength,min, ksi [Mpa] 95[655]
Yield Strength, min,ksi [MPa] 65[450]
Elongation in 2 in.[50 mm] or 4D,min, % 25
Reduction of Area, min, % 45
Brinell Hardness Number