ASTM A312 TP347

Spread the love

ASTM A312 TP347

Chemical Requirements:  Composition, %, max

Grade TP347(S34700)
Carbon 0.08
Manganese 2.00
Phosphorus 0.045
Sulfur 0.030
Silicon 1.00
Chromium 17.0-19.0
Nickel 9.0-13.0
Columbium 10*Carbon-1.00

 

Heat Treating Temperature: 1900 °F [1040 °C]

 

Tensile Requirements:

Tensile Strength, min ksi [MPa] 75 [515]
Yield Strength, min ksi [MPa] 30 [205]

 

Elongation in 2 in. or 50 mm (or 4D), min, %:

Longitudinal 35
Transverse 25